Romanian
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Guang Pu Xue Yu Guang Pu Fen Xi/Spectroscopy and Spectral Analysis 2010-Aug

[FTIR studies of masson pine wood decayed by brown-rot fungi].

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
Linkul este salvat în clipboard
Gai-yun Li
An-min Huang
Te-fu Qin
Luo-hua Huang

Cuvinte cheie

Abstract

Fourier transform infrared (FTIR) spectroscopy was used to study the chemical changes of masson pine (pinus massoniana lamb.) decayed by the brown-rot fungus Wolfiporia cocos (Schwein.) Ryvarden & Gilbn. for different durations up to 23 weeks. The ratios of height of the lignin/holocellulose and holocellulose/lignin IR peaks were measured, and the klason lignin content and holocellulose content of the sound wood and brown-rotted wood with different level of decay were analyzed by wet chemical methods. The relationship between the two chemical components and the ratios of IR peak height was also established. FTIR spectra showed that, during the first 15 weeks of decay, the intensity of absorption bands at 1 736 and 1 372 cm(-1) ascribed to holocellulose decreased gradually, accompanied by a successive increase in the intensity of band at 1 510 and 1 225 cm(-1) ascribed to lignin. However, the intensities of holocellulose bands at 1736 and 1372 cm(-1) had a little increase, and the intensities of lignin bands at 1 510 and 1 225 cm(-1) had a very slight decrease after 15 weeks of decay. There was a very good correlation between the ratios of height of the lignin/holocellulose (I1510/1736, I1510/I1372, I1225/I736 and I1225/I1372) and the klason lignin content or holocellulose content. The coefficients of determination for the klason lignin content and the holocellulose content were 0.97-0.99 and 0.96-0.97, respectively. High coeffieients of determination were also obtained between the holocellulose/ lignin peak height ratios and the holocellulose content (R2 = 0.96). The above results suggest that, in the system studied, the klason lignin content and holocellulose content of wood decayed to differnent levels could be determined with reasonable accuracy by the FTIR technology.

Alăturați-vă paginii
noastre de facebook

Cea mai completă bază de date cu plante medicinale susținută de știință

  • Funcționează în 55 de limbi
  • Cure pe bază de plante susținute de știință
  • Recunoașterea ierburilor după imagine
  • Harta GPS interactivă - etichetați ierburile în locație (în curând)
  • Citiți publicațiile științifice legate de căutarea dvs.
  • Căutați plante medicinale după efectele lor
  • Organizați-vă interesele și rămâneți la curent cu noutățile de cercetare, studiile clinice și brevetele

Tastați un simptom sau o boală și citiți despre plante care ar putea ajuta, tastați o plantă și vedeți boli și simptome împotriva cărora este folosit.
* Toate informațiile se bazează pe cercetări științifice publicate

Google Play badgeApp Store badge