Romanian
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)

tungsten/epuizare

Linkul este salvat în clipboard
Pagină 1 din 40 rezultate
An electromechanically-coupled micro-contact resistance measurement system is built to mimic the contact process during fatigue testing of nanoscale-thickness interconnects using multiple probe methods. The design combines an optical microscope, high-resolution electronic balance, and

Fatigue Resistant Bioinspired Composite from Synergistic Two-Dimensional Nanocomponents.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
Portable and wearable electronics require much more flexible graphene-based electrode with high fatigue life, which could repeatedly bend, fold, or stretch without sacrificing its mechanical properties and electrical conductivity. Herein, a kind of ultrahigh fatigue resistant graphene-based

Contact fatigue response of porcelain-veneered alumina model systems.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
Fatigue damage modes and reliability of hand-veneered (HV) and over-pressed (OP) aluminum-oxide layer structures were compared. Influence of luting cement thickness on mechanical performance was investigated. Sixty-four aluminum-oxide plates (10 × 10 × 0.5 mm) were veneered with hand built-up or

Influence of Adhesive Strength, Fatigue Strength and Contact Mechanics on the Drilling Performance of Diamond Coating.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
Adhesive strength of the coating significantly affects the lifetime of the coating. However, it is still inevitable for the coating, even with strong adhesive strength, to peel off from the substrate after working for a while. In this work, fatigue and wear behaviors were employed to analyze the

Effect of core thickness differences on post-fatigue indentation fracture resistance of veneered zirconia crowns.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
OBJECTIVE Despite the excellent esthetics of veneered zirconia crowns, the incidence of chipping and fracture of veneer porcelain on zirconia crowns has been recognized to be higher than in metal ceramic crowns. The objective of this investigation was to study the effect of selected variations in

Recrystallization and grain growth induced by ELMs-like transient heat loads in deformed tungsten samples.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
Tungsten has been chosen as the main candidate for plasma facing components (PFCs) due to its superior properties under extreme operating conditions in future nuclear fusion reactors such as ITER. One of the serious issues for PFCs is the high heat load during transient events such as ELMs and

Study on fracture of tungsten wire induced by acoustic cavitation at different hydrostatic pressures and driving electric powers

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
The near-solid wall multi-bubble cavitation is an extremely complex phenomenon, and cavitation has strong erosiveness. The melting point (about 3410 °C) of tungsten is highest among all pure metals, and its hardness is also very high (its yield strength is greater than 1 GPa). What would happen to

Measurement of Fracture Toughness of Pure Tungsten Using a Small-Sized Compact Tension Specimen.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
The evaluation of fracture toughness of pure tungsten is essential for the structural integrity analysis in a fusion reactor. Therefore, the accurate quantification of fracture toughness of tungsten alloys is needed. However, due to the inherent brittleness of tungsten, it is difficult to introduce

Surface Fatigue Behaviour of a WC/aC:H Thin-film and the Tribochemical Impact of Zinc Dialkyldithiophosphate.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
In wind turbine gearboxes, (near-)surface initiated fatigue is attributed to be the primary failure mechanism. In this work, the surface fatigue of a hydrogenated tungsten carbide/amorphous carbon (WC/aC:H) thin-film was tested under severe cyclic tribo-contact using PolyAlphaOlefin (PAO) and PAO +

Phase Exchange Driven Wake-Up and Fatigue in Ferroelectric Hafnium Zirconium Oxide Films.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
Ferroelectric hafnium zirconium oxide holds great promise for a broad spectrum of CMOS compatible and scaled microelectronic applications, including memory, low voltage transistors, and infrared sensors, among others. An outstanding challenge hindering implementation of this material is polarization
Continuous intramuscular stimulation of tibialis anterior (TA) was used to test the hypothesis that irregular trains of stimuli can increase force production and offset the magnitude of fatigue when compared with a continuous train of regular stimuli at an identical mean frequency (19 or 24 Hz). To

Influence of Antagonist Material on Fatigue and Fracture Resistance of Zirconia Crowns.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
This study investigates the influence of the most commonly used indenter materials on fatigue survival and fracture resistance of zirconia crowns. A total of 40 zirconia crowns were prepared using computer-aided design (CAD)/computer-aided manufacturing

Fatigue measurement system designed for a chalcogenide-based device using a homemade heater tip.

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
A fatigue measurement system is designed using a homemade tungsten (W) heater tip. This system is composed of a pulse generator and an atomic force microscope with the W heater tip attached. Also included are a parameter analyzer and control devices. The entire measurement process is controlled by a

[A comparative study on cyclic and static fatigue of dental ceramic by means of Hertzian's contact].

Numai utilizatorii înregistrați pot traduce articole
Log In / Înregistrare
OBJECTIVE To compare the difference in strength degradation and morphology damage of brittle dental ceramic after static load and cyclic fatigue. METHODS Hertzian's contact technique with a tungsten carbide sphere was used to investigate the response of feldspathic dental porcelain to static load
Caffeine increases time to fatigue [limit of endurance (T(lim))] during submaximal isometric contractions without altering whole muscle activation or neuromuscular junction transmission. We used 10 male volunteers in a randomized, double-blind, repeated-measures experiment to examine single motor
Alăturați-vă paginii
noastre de facebook

Cea mai completă bază de date cu plante medicinale susținută de știință

  • Funcționează în 55 de limbi
  • Cure pe bază de plante susținute de știință
  • Recunoașterea ierburilor după imagine
  • Harta GPS interactivă - etichetați ierburile în locație (în curând)
  • Citiți publicațiile științifice legate de căutarea dvs.
  • Căutați plante medicinale după efectele lor
  • Organizați-vă interesele și rămâneți la curent cu noutățile de cercetare, studiile clinice și brevetele

Tastați un simptom sau o boală și citiți despre plante care ar putea ajuta, tastați o plantă și vedeți boli și simptome împotriva cărora este folosit.
* Toate informațiile se bazează pe cercetări științifice publicate

Google Play badgeApp Store badge