Russian
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Journal of Biomedical Materials Research - Part B Applied Biomaterials 2012-Feb

Contact fatigue response of porcelain-veneered alumina model systems.

Только зарегистрированные пользователи могут переводить статьи
Войти Зарегистрироваться
Ссылка сохраняется в буфер обмена
Christian F J Stappert
Marta Baldassarri
Yu Zhang
Dina Stappert
Van P Thompson

Ключевые слова

абстрактный

Fatigue damage modes and reliability of hand-veneered (HV) and over-pressed (OP) aluminum-oxide layer structures were compared. Influence of luting cement thickness on mechanical performance was investigated. Sixty-four aluminum-oxide plates (10 × 10 × 0.5 mm) were veneered with hand built-up or pressed porcelain (0.7 mm) and adhesively luted (50- or 150-μm cement thickness) to water-aged composite resin blocks (12 × 12 × 4 mm). Single-load-to-failure and fatigue tests were performed with a spherical tungsten carbide indenter (d = 6.25 mm) applied in the center of the veneer layer. Specimens were inspected with polarized-reflected-light and scanning electron microscopy. Use-level probability Weibull curves were plotted with two-sided 90% confidence bounds, and reliability at 75,000 cycles and 250 N load was calculated. For all specimens but two OP with 50-μm cement thickness, failure was characterized by flexural radial cracks initiating at the bottom surface of the alumina core and propagating into the veneering porcelain before cone cracks could extend to the porcelain/alumina interface. HV specimens showed higher reliability compared to OP. Those with 50-μm cement thickness were more reliable relative to their 150-μm counterparts (HV_50 μm: 95% (0.99/0.67); HV_150 μm: 55% (0.92/0.01); OP_50 μm: 69% (0.84/0.48); OP_150 μm: 15% (0.53/0.004)). Similar failure modes were observed in HV and OP specimens. Radial cracks developing in the core and spreading into the veneer are suggested to cause bulk fracture, which is the characteristic failure mode for alumina core crowns. However, the highest resistance to fatigue loading was found for the HV specimens with thin cement thickness, while the lowest occurred for the OP with thick cement layer.

Присоединяйтесь к нашей
странице facebook

Самая полная база данных о лекарственных травах, подтвержденная наукой

  • Работает на 55 языках
  • Травяные лекарства, подтвержденные наукой
  • Распознавание трав по изображению
  • Интерактивная карта GPS - отметьте травы на месте (скоро)
  • Прочтите научные публикации, связанные с вашим поиском
  • Ищите лекарственные травы по их действию
  • Организуйте свои интересы и будьте в курсе новостей исследований, клинических испытаний и патентов

Введите симптом или заболевание и прочтите о травах, которые могут помочь, введите лекарство и узнайте о болезнях и симптомах, против которых оно применяется.
* Вся информация основана на опубликованных научных исследованиях.

Google Play badgeApp Store badge