Serbian
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Journal of the Mechanical Behavior of Biomedical Materials 2018-Dec

Precision of different fatigue methods for predicting glass-ceramic failure.

Само регистровани корисници могу преводити чланке
Пријави се / Пријави се
Веза се чува у привремену меморију
Rodrigo Ottoni
Jason A Griggs
Pedro H Corazza
Álvaro Della Bona
Márcia Borba

Кључне речи

Апстрактан

This study aimed to characterize the fatigue behavior using two fatigue methods, boundary and staircase, and to predict the probability of failure (Pf) of zirconia-reinforced lithium silicate glass-ceramic (ZLS). Bar-shaped specimens of ZLS (18 ×4 ×1.2 mm) were fabricated. Thirty specimens were subjected to a three-point flexural strength test using a universal testing machine with 0.5 mm/min crosshead speed, in 37 °C distilled water. Flexural strength data were analyzed with Weibull statistics. Eighty-six bars were subjected to cyclic fatigue using boundary and staircase methods. Fatigue tests were performed in a pneumatic cycling machine (2 Hz, 37 °C distilled water) for 10 ³ and 104 cycles. Fatigue data were analyzed using an inverse power law relationship and log normal-lifetime distribution. Fracture toughness (KIc) was determined using V-notched specimens (18 ×4 ×3 mm) and the short beam toughness method (n = 7). Vickers hardness (VH) was evaluated (4.9 N, 20 s). Fractographic and EDS analyses were also performed. ZLS showed a characteristic strength of 197 MPa, Weibull modulus of 4, VH of 6.67 GPa and KIc of 1.93 MPa m1/2. After 103 cycles, for both methods, there was a degradation of 78% of the initial strength. There was no significant degradation when the number of cycles increased from 103 to 104. Both methods resulted in similar Pf and precision at 40 MPa (~50% Pf). Yet, staircase shows good accuracy and precision in predicting the stress amplitude for a Pf near 50%; while boundary is also effective for Pf lower than 50%. The fatigue methods evaluated show similar accuracy and precision for predicting the Pf of a glass-ceramic when simulations were made in the range of stress levels and lifetimes used in the fatigue tests.

Придружите се нашој
facebook страници

Најкомплетнија база лековитог биља подржана науком

  • Ради на 55 језика
  • Биљни лекови потпомогнути науком
  • Препознавање биљака по слици
  • Интерактивна ГПС мапа - означите биље на локацији (ускоро)
  • Читајте научне публикације повезане са вашом претрагом
  • Претражите лековито биље по њиховим ефектима
  • Организујте своја интересовања и будите у току са истраживањем вести, клиничким испитивањима и патентима

Упишите симптом или болест и прочитајте о биљкама које би могле да помогну, укуцајте неку биљку и погледајте болести и симптоме против којих се користи.
* Све информације се заснивају на објављеним научним истраживањима

Google Play badgeApp Store badge