中文(繁體)
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Applied and Environmental Microbiology 1990-Jun

Comparative studies of delignification caused by ganoderma species.

只有註冊用戶可以翻譯文章
登陸註冊
鏈接已保存到剪貼板
J E Adaskaveg
R L Gilbertson
R A Blanchette

關鍵詞

抽象

Isolates of six species of Ganoderma in the G. lucidum complex were evaluated for their ability to decay wood of Quercus hypoleucoides A. Camus and Abies concolor (Gord. and Glend.) Lindl. ex. Hildebr. by using in vitro agar block decay tests. Morphological, ultrastructural, and chemical studies of decayed wood were used to determine the extent of delignification or simultaneous decay caused by each species of Ganoderma. All species decayed both white fir and oak wood; however, less percent weight loss (%WL) occurred in white fir than oak. In white fir, isolates of two undescribed Ganoderma species (RLG16161, RLG16162, JEA615, and JEA625) caused significantly higher%WL (21 to 26%) than that in G. colossum, G. oregonense, G. meredithiae, and G. zonatum (10 to 16%). Only Ganoderma sp. isolates JEA615 and JEA625 caused delignification, with JEA615 causing a lignin-to-glucose gram loss ratio of 1.6:1. Morphological and ultrastructural studies confirmed delignification by this fungus and showed that some delignification had occurred by all of the species, although areas of delignification were limited to small regions adjacent to simultaneously decayed cells. In oak, G. colossum caused significantly less%WL (22 to 35%) than the other species (38 to 52%). All of the species, except G. meredithiae, caused delignification with lignin-to-glucose gram loss ratios ranging from 1.4 to 4.9:1. Extensive delignification by isolates of G. colossum and G. oregonense was observed; moderate delignification was caused by the other species. Ganoderma meredithiae caused a simultaneous decay, with only small localized regions of cells delignified, while delignification by G. zonatum was irregular, with specific zones within the cell wall delignified. The thermophilic and chlamydosporic G. colossum has the capacity to cause extensive delignification and appears ideally suited for use in lignin degradation studies and biotechnological applications of lignin-degrading fungi.

加入我們的臉書專頁

科學支持的最完整的草藥數據庫

  • 支持55種語言
  • 科學支持的草藥療法
  • 通過圖像識別草藥
  • 交互式GPS地圖-在位置標記草藥(即將推出)
  • 閱讀與您的搜索相關的科學出版物
  • 通過藥效搜索藥草
  • 組織您的興趣並及時了解新聞研究,臨床試驗和專利

輸入症狀或疾病,並閱讀可能有用的草藥,輸入草藥並查看其所針對的疾病和症狀。
*所有信息均基於已發表的科學研究

Google Play badgeApp Store badge